Description: THERMODAN® CP 0110-108 BKm is a black, UV resistant, lead-free, RoHS compliant, thermoplastic CPE compound. It is designed for use in a wide variety of jacketing applications including wire and cable and tube bundles. This compound has superior fire performance including slow flame propagation and self-extinguishing characteristics. THERMODAN® CP 0110-108 BKm should be extruded with a screw configuration designed to optimize process conditions and throughput. This extrusion compound meets or exceeds several industry jacketing specifications including UL 1277 tray cable.Information provided by SACO AEI Polymers. |