MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Moplen HP640G Sheet and Thermoforming Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Moplen HP640G is the polypropylene Homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640G is a homopolymer particularly suitable for sheet and thermoforming. Moplen HP640G resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.

Features: Excellent processability and stretchability; High stiffness; High heat distortion temperature; High mechanical properties; Excellent melt strength

Applications: Food packaging and tray; Rigid sheet; Microwave-use

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 1.25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.25 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 38.2 MPa5550 psiASTM D638
Elongation at Yield 11 %11 %ASTM D638
Flexural Modulus 1.67 GPa242 ksiASTM D790
Izod Impact, Notched 0.588 J/cm1.10 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FASTM D648
Vicat Softening Point 158 °C316 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accucomp Polypropylene HPO306L Homopolymer
Envalior EcoPaXX® Q-KV PA410 FR, Dry, Flame Retardant
Aclo Accutech Polypropylene CP0437T40V Copolymer Talc Reinforced
Aclo Accutech Polypropylene CP0435G20HIV Copolymer Glass Reinforced High Impact
Aclo Accutech Polypropylene CP0409HUUVV Copolymer UV Stabilized

PMIRAE52 / 53164

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.