MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond NPP 60-1300 GF30 30% Glass Filled Polyester Alloy
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Polyester Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Filler Content 28 - 32 %Glass Fiber; ASTM D5630
Viscosity 1.20e+6 cP
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
Linear Mold Shrinkage 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 103.5 MPachs 2.0 in/min; ASTM D638
Flexural Modulus 6486 MPachs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 80.0 J/m
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond DIAMALOY 508 30% Glass Filled PC/Polyester Alloy, UV Stabilized
MetalTek WCB UNS J13345 Cast Alloy Steel
American Polymers API 375 Polystyrene
A. Schulman TPP40AC46BK 40% Talc Filled, Heat Stabilized, Homopolymer Polypropylene
A. Schulman TPP20AC06HB 20% Talc Filled, Heat Stabilized, Homopolymer Polypropylene

PDIAM471 / 126562

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.