MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil PP7033E2 Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: A high crystallinity, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate.

Availability: North America and Asia Pacific

Features:

  • Good Colorablity
  • Good Dimensional Stability
  • Medium Flow
  • Medium Impact Resistance
Uses:
  • Automotive Applications
  • Automotive Interior Parts
  • Automotive Interior Trim
  • Child Safety Seats
  • Consumer Applications
  • Toys
Processing Method: Injection Molding

Automotive Specifications: Hyundai MS213-24 Type 6

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3600 psi2 in/min; ASTM D638
Elongation at Yield 6.4 %2 in/min; ASTM D638
Flexural Modulus, 1% Secant 163000 psi0.05 in/min; ASTM D790
 189000 psi0.05 in/min; ASTM D790B
Izod Impact, Notched 4.30 ft-lb/inASTM D256
Gardner Impact 211 in-lb
@Thickness 3.17 mm,
Temperature -30.0 °C
ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 204 - 246 °CTypical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP7033N Impact Copolymer
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7060-1000 TPE
ExxonMobil PP7032E2 Impact Copolymer
Avient Maxxam™ PD 20 TF Black Polypropylene
ExxonMobil PP7033L1 Polypropylene Impact Copolymer

PEXB284 / 37589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.