MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax™ CA10GC Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ CA10GC fractional melt flow, 100 MPa flexural modulus, precolored, UV-stabilized, reactor grade, extrudable thermoplastic elastomeric olefin (TEO) resin combines good processability with balanced strength, toughness, flexibility and weatherability. It is based on material produced from proprietary Basell process technology and was designed primarily for applications requiring extended outdoor exposure. Uses: Sheet, geo membranes

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.892 g/ccASTM D792
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 43ASTM D2240
Tensile Strength at Break 2030 psiASTM D 638
Tensile Strength, Yield 1310 psiASTM D 638
Elongation at Break 600 %ASTM D 638
Flexural Modulus 13100 psiTangent, 0.05 in/min; ASTM D790
 14500 psiTangent, 0.5 in/min; ASTM D790
Tear Strength 450 pliASTM D624

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hifax™ CA45 Thermoplastic Olefin Resin
LyondellBasell Hifax™ CA387 Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CA287AHF Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CA244 Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CA207A Thermoplastic Polyolefin Elastomer

PMO775 / 53764

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.