MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MetalTek NAVY G 1% LEAD Cast UNS C92300 Bearing Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.

Applications: Worm gears, steel mill nuts

Information provided by MetalTek

Cast UNS C92300; Cast Grade C92300; Cast ASTM B271, B584; Military MIL-C-15345-10; SAE 621 (Discontinued)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.64 g/ccBased on UNS number
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 75500 kg
Tensile Strength, Ultimate >= 250 MPa
Tensile Strength, Yield >= 110 MPa
Elongation at Break >= 18 %
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 87 %
Lead, Pb 1.0 %
Tin, Sn 8.0 %
Zinc, Zn 4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek NAVY G Cast UNS C90300 Bearing Bronze
MetalTek NAVY M Cast UNS C92200 Bearing Bronze
Mueller Dynalloy Alloy 6730 Free cutting bearing bronze (UNS C67300)
MetalTek BeariumĀ® B-11 Bearing Bronze
MetalTek MTEK 80-10-10 Cast UNS C93700 Bearing Bronze

NMETEK030 / 18280

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.