MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.

Key applications for Akulon:

  • Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectors
  • Consumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, Transportation
  • E&E: Low voltage switch gear/power distribution, Lighting, Power connectors
  • Film: Specialty and barrier films

Information provided by DSM.

Akulon is a former DSM Engineering Plastics product line now with Envalior, although this specific product was discontinued prior to that transaction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccISO 1183
Water Absorption 4.5 %Sim. to ISO 62
Moisture Absorption at Equilibrium 1.3 %Humidity Absorption; Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPaISO 527-1/-2
Elongation at Break 2.5 %ISO 527-1/-2
Tensile Modulus 11.5 GPaISO 527-1/-2
Charpy Impact Unnotched 6.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 6.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 1.30 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.4
@Frequency 1e+6 Hz
IEC 60250
 3.5
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0060
@Frequency 100 Hz
IEC 60250
 0.012
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 425 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-1/-2
Flammability, UL94 V-0
@Thickness 1.60 mm
IEC 60695-11-10
 V-0
@Thickness 0.750 mm
IEC 60695-11-10
 
Descriptive Properties
Flame RetardantYes
Flame Retarding AgentYes
Heat Stabilized or Stable to HeatYes
Injection MoldingYes
With FillersYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® Ultraflow K-FKGS6/B PA6-GF30 FR(17), Dry, 30% Glass Filled, Heat Stabilized, Flame Retardant
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)
Envalior Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17)
Akro-Plastic Akroloy® PA GF 30 (2718) PA 6.6 & PA6I/6T Dry, 30% Glass Filled
Envalior Akulon® XG-FKGS6 PA6-GF30 FR

PDSMEU294 / 31268

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.