MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kennametal Stellite Stellite® 19
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Can be machined with carbide tipped tools, but when hardness exceeds Rc55 it is best to grind. Applications include cutting tools, bearing races, guide rolls, and nozzle discs. Excellent resistance to hot abrasion and adhesive wear, low coefficient of friction. Resistant to atmospheric oxidation and forms only a thin adherent scale at red heat. Resists attack from wet chlorine and acetic acid (boiling), excellent resistance to 10% boiling nitric, and 10% sulfuric acid at room temperature. Fair resistance to concentrated nitric boiling and 10% boiling sulfuric. Poor resistance to 77% sulfuric boiling and reducing acids. Data provided by the manufacturer, Deloro Stellite, Inc.

Product of former Deloro Stellite Inc.

Key Words: MIL-C-24248 Comp II
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.36 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 45 - 60
Tensile Strength, Ultimate 724 MPa(Tensile Yield Strength near U.T.S.)
Elongation at Break <= 1.0 %
Modulus of Elasticity 234 GPa
Ultimate Compressive Strength 2137 MPa
Izod Impact Unnotched 4.75 J
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.8 µm/m-°C
@Temperature 20.0 - 100 °C
 13.7 µm/m-°C
@Temperature 20.0 - 300 °C
 14.2 µm/m-°C
@Temperature 20.0 - 500 °C
 14.2 µm/m-°C
@Temperature 20.0 - 600 °C
 14.8 µm/m-°C
@Temperature 20.0 - 700 °C
 15.1 µm/m-°C
@Temperature 20.0 - 800 °C
 16.9 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 14.7 W/m-K
Melting Point 1239 - 1299 °C
Solidus 1239 °C
Liquidus 1299 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.8 %
Chromium, Cr 31 %
Cobalt, Co 52.2 %As remainder
Iron, Fe 2.5 %
Nickel, Ni 1.0 %
Silicon, Si 1.0 %
Tungsten, W 10.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 190 PM with P/M Processing
Kennametal Stellite Stellite® 12
Kennametal Stellite Stellite® 3 PM cast
Kennametal Stellite Stellite® 21
Kennametal Stellite Stellite® 12 PM with P/M Processing

NSTA19 / 19245

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.