MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.

Benefits: The product offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature. The product offers an improved hydrolisis resistance, as well as an excellent combination between thermal and mechanical properties. It also restricts electrolytical corrosion.

Available in: Asia Pacific and Europe

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This grade is recommended for the production of mechanical components in permanent or intermittent contact with hot water, such as electro-magnetic valves. It can also be used as insulation material for electronic connectors, due to its limited electrolytical corrosion.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183/A
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Viscosity 120 cP
@Shear Rate 100 1/s,
Temperature 290 °C
 150 cP
@Shear Rate 100 1/s,
Temperature 280 °C
 200 cP
@Shear Rate 100 1/s,
Temperature 270 °C
 205 cP
@Shear Rate 10 1/s,
Temperature 290 °C
 300 cP
@Shear Rate 10 1/s,
Temperature 280 °C
 500 cP
@Shear Rate 10 1/s,
Temperature 270 °C
Linear Mold Shrinkage 0.0062 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPaISO 527 Type 1A
Tensile Stress at Strain 85.0 MPa
@Strain 1 %
 155 MPa
@Strain 2 %
 180 MPa
@Strain 3 %
Elongation at Break 3.2 %ISO 527 Type 1A
Tensile Modulus 10000 MPaISO 527 Type 1A
Flexural Strength 270 MPaISO 178
Flexural Modulus 8600 MPaASTM D790
 9000 MPaISO 178
Izod Impact, Notched 105 J/mASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 85.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 3.7IEC 60250
Dielectric Strength 35.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
CTE, linear, Transverse to Flow 28.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 262 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °CASTM D648
 254 °CISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
1210
Glow Wire Flammability Index 700 °C
@Thickness 1.60 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 275 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, Conditioned
Domo TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, Conditioned
Domo TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Domo Technyl® A218 Heat Stabilized Nylon 66

PRHOD680 / 137911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.