Hostacom EKC 330NA NATURAL high melt flow, medium high flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent impact/stiffness balance, good flowability properties and excellent scratch resistance. It is typically used for interior automotive applications. Applications: Automotive Parts, Interior Automotive ApplicationsInformation provided by LyondellBasell. |