MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
TIMET TIMETAL® 6-4 Titanium Alloy (Ti-6Al-4V-0.1Ru; ASTM Grade 29)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Medium To High Strength General-Purpose Alloy. Property data below are typical of Timet® 6-4 ELI (without Ru). The 0.1 Ru ELI variant is used for enhanced corrosion resistance.

Data provided by TIMET.

Key Words: Titanium 6-4
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.42 g/ccTypical
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 897 MPaTypical
Tensile Strength, Yield 828 MPa
@Strain 0.2 %
Typical
Elongation at Break 16 %Typical
Modulus of Elasticity 95.0 - 111 GPa
@Temperature 230 °C
varies with heat treatment and texture
 107 - 122 GPa
@Temperature 20.0 °C
varies with heat treatment and texture
Poissons Ratio 0.31
Shear Modulus 41.0 - 45.0 GPa
Bend Radius, Minimum 5.0 tTypical; on 0.078 in (2 mm) sheet
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000168 ohm-cm
 0.000168 ohm-cm
@Temperature 0.000 °C
 0.000186 ohm-cm
@Temperature 315 °C
 0.000189 ohm-cm
@Temperature 650 °C
Magnetic Permeability 1.00005at 20 Oersted
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µm/m-°C
@Temperature 0.000 - 100 °C
 9.40 µm/m-°C
@Temperature 20.0 - 425 °C
 9.70 µm/m-°C
@Temperature 20.0 - 650 °C
Specific Heat Capacity 0.580 J/g-°C
@Temperature 20.0 °C
 0.670 J/g-°C
@Temperature 425 °C
 0.930 J/g-°C
@Temperature 870 °C
Thermal Conductivity 6.60 W/m-K
@Temperature 20.0 °C
 10.6 W/m-K
@Temperature 315 °C
 17.5 W/m-K
@Temperature 650 °C
Melting Point <= 1660 °C
Liquidus >= 1636 °C
 1660 °C
Maximum Service Temperature, Air 350 °CReasonable mechanical properties retained
Beta Transus 982 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.5 - 6.5 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.25 %
Nitrogen, N <= 0.030 %
Other, each <= 0.10 %
Other, total <= 0.40 %
Oxygen, O <= 0.13 %
Ruthenium, Ru 0.080 - 0.14 %
Titanium, Ti 88 - 90.9 %Calculated as remainder
Vanadium, V 3.5 - 4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-4V (Grade 5), STA
Titanium Ti-6Al-4V (Grade 5), Annealed
Titanium Ti-6Al-4V ELI (Grade 23), Annealed
Titanium Grade 29 Ti-6Al4V-0.5Ru
Titanium Grade 24 Ti-6Al-4V-0.06Pd

NTIME64RU / 19332

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.