MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Filler Content 13 %Carbon Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 78.6 MPaASTM D638
Elongation at Break 1.5 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 7720 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 123 MPaASTM D790
Flexural Modulus 8620 MPaASTM D790
Izod Impact, Notched 43.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 ohm-cm - 1e+05ASTM D257
Surface Resistance 1000 ohm - 1e+05ASTM D257
Static Decay 0.0020 sec(Mil-B-81705C), 12% RH, 5000 kV to 50 kV
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Flammability, UL94 HBInternal Method
 
Processing PropertiesOriginal ValueComments
Melt Temperature 227 - 238 °C
 
Descriptive Properties
FeaturesAntistatic
 Conductive
 Electrically Conductive
 Statically Conductive
FormsPellets
Generic MaterialABS
Generic NameAcrylonitrile Butadiene Styrene (ABS)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesComputer Components
 Connectors
 Electrical Housing
 Electrical/Electronic Applications
 Housings
 Medical Device Housings
 Medical/Healthcare Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
LG Chemical HF380G ABS, High Flow
Elix Polymers Elix™ DP M116GF ABS Polymer
Covestro Makrofol® DE 1-4 000000 Polycarbonate
Avient Trilliant™ HC HC6600-0010 ESD Black Polyamide 66 (Nylon 66)

PH0POL1293 / 145862

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.