MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
OJSC Plastic ABS 2020-31 M ABS Plastic
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Injection molding grade.

Pellet Size: granulates from 2 mm to 5 mm in size in any direction. No more than 1% of granules from 5mm to 8mm in size and no more than 1% of granules from 1mm to 2mm size are allowed. Clearness of disk surface: inclusions no more than one point no more than 0.3mm in size on a surface of a disk if 10cm² are allowed.

Information provided by manufacturer.

Key Words: TU 2214-019-0020352196
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cmunder pressure
Melt Flow 12 - 16 g/10 min
@Load 10.0 kg,
Temperature 220 °C
GOST 11645
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 35.3 MPasample-shovel type II, 20±2 mm/min; GOST 11262
Elongation at Break 22 %paddle type II, 20±2mm.
Izod Impact, Notched (ISO) >= 24.5 kJ/m²sample type 1, with cut 3.2mm; GOST 19109
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 98.0 °Cannealed, sample 127x12.7x3.2, T=100±2°C, 2 hours
Vicat Softening Point >= 97.0 °Cload 50N; 120°C/hour; GOST 15088
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.30 %TU 2214-044-05762341-2015, change 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
OJSC Plastic ABS 2020-31 ABS Plastic
OJSC Plastic ABS 1530-32 ABS Plastic
Sibur ABS 1530 Molding Grade ABS Plastic
Kleerdex Elson® 407AS DC Plate, Polycarbonate, Clear
3D Systems Fused Deposition Modeling Material ABS

POJSC951 / 192473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.