MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane ethylene homopolymers with comparable density.

Applications:
• Supporting material for compounds
• Polymer modification of bitumen and asphalt
• Powder coating
• Rotomolding

Information provided by Lucobit AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccISO 1183
Particle Size 500 µmASTM D 1921
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88ISO 868
Hardness, Shore D 32ISO 868
Tensile Strength, Yield 3.50 MPaISO 527
Elongation at Yield 13 %ISO 527
Modulus of Elasticity 0.0450 GPaISO 527
 
Thermal PropertiesOriginal ValueComments
Melting Point 95.0 °CISO 3146
Vicat Softening Point 60.0 °CISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 220 °CRotomolding
 160 - 240 °CBitumen modification
 160 - 270 °CCoatings
 160 - 290 °CCompounding
 
Descriptive Properties
Comonomer BA0.17DIN 51451

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate
Arkema LOTRYL® 35 BA 40 Copolymer Ethylene - Butyl Acrylate
Arkema LOTRYL® 35 BA 320 Copolymer Ethylene - Butyl Acrylate
Dow Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate

PLUCO916 / 150982

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.