MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M E-FIS Fire Barrier Expantrol Flexible Intumescent Strip
Categories: Polymer

Material Notes: 3M Fire Barrier E-FIS has been designed to seal the air space between doors and frames and for glazing fire resistant glass to help prevent the passage of smoke and flames in the event of a fire. When exposed to heat such as would occur in a fire, the material expands to seal the gap and forms a char to deter the spread of a fire. This expansion or intumescence of the material helps prevent noxious gases, flames or other by-products that may be produced in a fire from penetrating into adjacent areas.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8181
Tensile Strength at Break 1.99 MPa289 psiASTM D412-83
Elongation at Break 903 %903 %ASTM D412-83
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.410 W/m-K
@Thickness 3.17 mm,
Temperature 66.0 °C
2.85 BTU-in/hr-ft²-°F
@Thickness 0.125 in,
Temperature 151 °F
ASTM C518
 0.410 W/m-K
@Thickness 3.17 mm,
Temperature 86.0 °C
2.85 BTU-in/hr-ft²-°F
@Thickness 0.125 in,
Temperature 187 °F
ASTM C518
 0.420 W/m-K
@Thickness 3.17 mm,
Temperature 47.0 °C
2.91 BTU-in/hr-ft²-°F
@Thickness 0.125 in,
Temperature 117 °F
ASTM C518
 
Descriptive Properties
AppearanceRed-Brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35451 / 170198

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.