MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe BG42® Stainless Knife Steel (AMS 5749)
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel

Material Notes: LESCALLOY® BG42® VIM VAR is a double vacuum melted martensitic stainless high speed steel designed for critical aerospace structural components and high performance bearings. The steel is vacuum induction melted (VIM) and vacuum arc remelted (VAR) to provide the extremely high cleanliness level required for these fatigue-critical applications. When manufactured in sheet form, BG42 has proven to be an excellent knife steel. The very good wear resistance and corrosion resistance result in knife blades which exhibit excellent edge retention and long life. The molybdenum in the steel enhances the corrosion resistance provided by the high chromium content. In addition, the chromium, molybdenum, and vanadium contents provide approximately 19% carbide volume in the steel. This high carbide volume and the presence of very hard vanadium carbides enhance the wear resistance and edge retention of knife blades. The excellent edge retention and good corrosion resistance establish BG42 as an upgrade material compared to the

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.75 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 59Oil Quenched from 1149°C, 10 minutes
 59.5Oil Quenched from 1066°C, 15 minutes
 62.5Oil Quenched from 1093°C, 15 minutes
Modulus of Elasticity 180.6 GPa
@Temperature 482 °C
 220.6 GPa
@Temperature 22.2 °C
Modulus of Rigidity 70.4 GPa
@Temperature 482 °C
 86.53 GPa
@Temperature 22.2 °C
Poissons Ratio 0.27
@Temperature 22.2 °C
Machinability 55 - 60 %1% Carbon Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.45 µin/in-°F
@Temperature -73.3 - 21.1 °C
 6.13 µin/in-°F
@Temperature 21.1 - 149 °C
 6.85 µin/in-°F
@Temperature 21.1 - 538 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.15 %
Chromium, Cr 14.5 %
Iron, Fe 78.35 %
Manganese, Mn 0.50 %
Molybdenum, Mo 4.0 %
Silicon, Si 0.30 %
Vanadium, V 1.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe Lescalloy® BG42 VIM-VAR High Performance Bearing Steel
Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel
AISI 440 Stainless Steel
AK Steel 201 Austenitic Stainless steel
ATI Allvac® M-50 Specialty Steel, Heat Treatment: 1107°C (2025°F) Q+T

NTIMK136 / 19483

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.