MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Coating P. Materials CL-165FR Calendering Grade TPU for Eco-friendly Synthetic Leather
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: CPMC specializes in developing TPU applicable for calendaring. It has good physical; Good melt; Good transparency; Good flexibility; Excellent abrasion resistance; Good workability; Low gel content; Well low-temperature flexibility. It’s applicable for conveyor belt, sheet and film, air cushion, protection sleeve, extrusion, profile extrusion, melt coatings on textile substrates, belting, by extrusion.

Product Description: Good physical, good melt, good transparency, good flexibility, high abrasion resistance and good workability.

Application To End-Use Products: Conveyor belt, sheet and film, air cushion, protection sleeve, extrusion, profile extrusion.

Information provided by Coating P. Materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 67 - 7367 - 73ASTM D2240
Tensile Strength 8.83 MPa1280 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
100% Modulus 3.92 MPa569 psiASTM D412
300% Modulus 6.37 MPa925 psiASTM D412
 
Descriptive Properties
CharacteristicFlame-retardant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTCOAT006 / 293950

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.