MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
St. Cloud Natural Zeolite (Clinoptilolite)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large internal surface area in the porous structure and exchangable cations lead to a variety of uses. It is used as an animal feed supplement that has been shown to improve health and reduce the negative effects of animal waste; as an additive to animal stalls and pens to reduce ammonia and other emissions to air and water; as a soil amendment to retain water and plant nutrients in root zones, which conserves both; for a number of other horticultural and agricultural uses, including being endorsed for use in space by NASA; as a water filtration media that removes ammonia, some heavy metals and other constituents; etc.

Major exchangeable cations are Rb, Li, K, Cs, NH4, Na, Ca, Ag, Cd, Pb, Zn, Ba, Sr, Cu, Hg, Mg, Fe, Co, Al, Cr. Primary adsorbing gases are CO, CO2, SO2, H2S, NH3, HCHO, Ar, O2, N2, H2O, He, H2, Kr, Xe, CH2OH, Freon, formaldehyde, and mercaptans.

Product mined near Winston, New Mexico, USA.

Information provided by St. Cloud Mining Company.

Key Words: (Ca, Na2, K2)(Al6 SiO)-24H2O; Calcium-sodium-potassium aluminosilicate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.20 - 2.40 g/cc
Bulk Density 44.0 - 48.0 lb/ft³Aggregate, dried, 4 x 6 mesh
 45.0 - 47.0 lb/ft³Aggregate, dried, 6 x 14 mesh
 46.0 - 49.0 lb/ft³Aggregate, dried, 14 x 40 mesh
 48.0 - 52.0 lb/ft³Aggregate, dried, -40 mesh
 87.0 lb/ft³In Place, dried
Porosity <= 52 %Natural Internal Porosity
pH 7.5 - 8.0Natural
Specific Surface Area 14 - 15 m²/gExternal
 <= 800 m²/gTotal
Permeability 0.001m/sec (1.4 - 0.4 mm particles)
Pore Size 0.000400 - 0.000700 microns4 - 7 angstroms Diameter
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 3.5 - 4.0
Compressive Strength 2500 psicrush strength
Abrasion 24LA Wear
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 9000 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 650 °C
 
Optical PropertiesOriginal ValueComments
Reflection Coefficient, Visible (0-1) 0.85
 
Component Elements PropertiesOriginal ValueComments
Al2O3 12.1 %
CaO 3.4 %
Fe2O3 1.6 %
K2O 3.0 %
MgO 1.5 %
Na2O 0.3 %
P2O5 0.05 %
SiO2 70 %
 
Descriptive Properties
Cation Exchange Capacity0.1 meq/g external
 0.8 – 1.2 meq/g total
Clinoptilolite Content75 to 85%
ColorWhite
Featurefree flowing
 non-slaking
 non-soluble
 readily mixable
pH Stability0 - 13
Si:Al Ratio5:1
Surface Charge Density10.1E-23 meq/Å2
Swelling Indexnil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Formaldehyde (HCHO; Methanal)
Honeywell Acetone Laboratory Plus
Diamond, Natural
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer
MarkeTech PWO (Lead tungstate, PbWO4) Scintillator Crystal

CSTCLO90 / 150051

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.