MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
FiberNide Nickel Aluminide Foam Atomic 22% Aluminum  (discontinued **)
Categories: Metal; Intermetallic; Metal Foam, Mesh, or Honeycomb; Metal Matrix Composite; Nonferrous Metal; Nickel Alloy; Other Engineering Material; Composite Core Material

Material Notes: Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable for a wide range of catalyst supports, combustion mantels, and heaters. The ability to bond to other metallic materials allows the foam to be used as foam cores in high temperature metallic composites, high temperature heat exchangers, and probably for cooled surfaces for hypersonic vehicles. Results apply to nickel aluminide foam formed from 0.4 mm pore size, 0.28 g/cc nickel foam. The mechanical properties of the nickel aluminide foam are expected to increase as the density of nickel aluminide foam increases and as the pore size increases.

Information provided by FiberNide, Ltd..

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 g/ccNi Foam Starting Material
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 5.52 - 5.53 MPa
Flexural Modulus 0.01492 - 0.01494 GPa
Compressive Yield Strength 2.91 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000330 - 0.000340 ohm-cmUnsintered
 0.000645 - 0.000655 ohm-cmSintered
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 11 %
Nickel, Ni 89 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cymat A35620SC 040SS Stabilized Aluminum Foam
FiberNide Nickel Foam
ERG Aerospace Duocel® Aluminum Metal Foam
FiberNide Nickel Aluminide Foam Atomic 10% Aluminum
FiberNide Nickel Aluminide Foam Atomic 20% Aluminum

NF04 / 16190

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.