MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials FRV1106 Red Fluorosilicone Adhesive Sealant, Fuel Resistant Paste
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: One-part acetoxy cure. Alkoxy cure silicones are neutral cure materials that offer exceptional adhesion and are non-corrosive to most metals. Typical uses: For use in contact with fuel, solvents, and chemicals.

Data provided by the manufacturer, GE Silicones.

GE Silicones became a part of Momentive Performance Materials in 2006.

Key Words: RTV Silicones; R.T.V. Silicones
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 42
Tensile Strength, Ultimate 3.33 MPa
Elongation at Break 230 %
Adhesive Bond Strength 1.38 MPaTypical lap shear
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.3
@Frequency 1000 Hz
Dielectric Strength 13.7 kV/mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 205 °CContinuous useful temperature.
Minimum Service Temperature, Air -60.0 °CContinuous useful temperature.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 25.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Rogers Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier
Momentive Performance Materials RTV159 Red Adhesive Sealant, High Strength Paste
Dow Silastic® LS 4-9038 FLUOROSILICONE RUBBER

PZZGE928 / 40482

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.