MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow LIGHTER™ C88 Polyethylene Terephthalate (PET) Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: LIGHTER™ resins are polyethylene terephthalate produced from PTA and MEG. These polymers are specifically designed for the production of beverage, food and other liquid containers and for thermoforming.

LIGHTER™ C88 is particularly suitable for bottling mineral water since it was designed to minimize the formation of acetaldehyde. In general this grade is recommended for bottles for both still and carbonated mineral water. It is also suitable for the production of extruded thermo formable sheets.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.880 g/cc1/MA/1/008
Viscosity Test 74 - 78 cm³/gIntrinsic Viscosity; 1/MA/1/002
 88 cm³/gISO Viscosity Number; ISO 1628/5
Crystallinity >= 50 %1/MA/1/018
 
Thermal PropertiesOriginal ValueComments
Melting Point 247 °Cpeak; 1/MA/1/007
Glass Transition Temp, Tg 78.0 °C1/MA/1/007
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.40 %1/MA/1/005
 
Descriptive Properties
Acetaldehyde ppm, max11/MA/1/004
Color, coordinate b, Max11/MA/1/003
Fine Particles Content ppm, max5001/MA/1/001
Weight of 100 Granules g1.51/MA/1/015

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow LIGHTER™ S98 Polyethylene Terephthalate (PET) Resin
Dow LIGHTER™ C93 Polyethylene Terephthalate (PET) Resin
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Dow LIGHTER™ S93 Polyethylene Terephthalate (PET) Resin
DAK Americas Laser+® C91A PET

PDOW1493 / 30711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.