MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Havoline® ATF+3® Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Havoline Automatic Transmission Fluid ATF+3 delivers value through:
  • Correct viscosity and frictional characteristics to ensure smooth operation in Chrysler transmissions.
  • Long-lasting viscosity modifiers for longer fluid life.

Havoline Automatic Transmission Fluid ATF+3 is designed specifically for use in Chrysler® automatic transmissions and automatic transaxles where a Mopar ATF PLUS®, ATF+2® or ATF+3® fluid is specified.

Havoline Automatic Transmission Fluid ATF+3 is designed to maintain its viscosity through excellent oxidation stability and use of long lasting viscosity modifiers.

It has improved low temperature fluidity and viscosity breakdown performance over previous generation Chrysler ATF fluids.

Havoline Automatic Transmission Fluid ATF+3 is specially formulated to give full protection in all critical areas of Chrysler transmission operation.

Havoline Automatic Transmission Fluid ATF+3:

  • Lubricates and prevents wear in gears, clutches, and bearings.
  • Transfers engine power effectively
  • Serves as a hydraulic fluid for the shift control system
  • Removes heat efficiently
  • Operates well over a wide temperature range
  • Resists thermal and oxidative breakdown
  • Provides sufficient viscosity at high temperatures with minimal sheardown
  • Gives proper friction performance for Chrysler vehicles (smooth shift feel, no shudder)
  • Protects seals, gaskets, and other nonferrous components
  • Prevents sludge and varnish formation
  • Resists foaming

Havoline Automatic Transmission Fluid ATF+3 is designed for use in all Chrysler automatic transmissions and automatic transaxles where a Mopar ATF PLUS, ATF+2 or ATF+3 fluid is specified.

It is not recommended for use in transmissions specifying either DEXRON® or MERCON® type fluids2.

Havoline Automatic Transmission Fluid ATF+3 has been registered with the Chrysler Corporation.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Chrysler, Mopar ATF PLUS, ATF+2, and ATF+3 are registered trademarks of DaimlerChrysler.
  2. DEXRON is a registered trademark of General Motors Corporation.
  3. MERCON is a registered trademark of Ford Motor Company.

CPS Number: 221803; MSDS Number: 8630

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31.2 °
Brookfield Viscosity 18000 cP
@Temperature -40.0 °C
Viscosity Measurement 188Viscosity Index
Kinematic Viscosity at 40°C (104°F) 35.9 cSt
Kinematic Viscosity at 100°C (212°F) 7.6 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °C
Flash Point 194 °C
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WTEXA071 / 76950

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.