MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petropol Unipren® A3 NTLA010 65A XP11 UP323 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Product Description: 65 Shore A, Elastomer

Resin ID (ISO 1043): TPE
Additive: PP / PE adhesion
Processing: Injection Molding, Extrusion
Color: Natural

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 62 - 6862 - 68ASTM D2240
Tensile Strength 7.00 MPa1020 psiASTM D412C
Elongation at Yield >= 600 %>= 600 %ASTM D412C
Tensile Modulus  0.00200 GPa
@Strain 100 %
0.290 ksi
@Strain 100 %
ASTM D412C
 0.00300 GPa
@Strain 300 %
0.435 ksi
@Strain 300 %
ASTM D412C
Tear Strength 40.0 kN/m229 pliASTM D624C
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 200 °C356 - 392 °FMolding
Mold Temperature 40.0 °C104 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL432 / 313340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.