MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Telcar® TL-4129 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TL-4129 is a low density thermoplastic elastomer designed for the industrial market. It is a clear TPE that is UV stable and that is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Light Stabilized; Low Density; Low Specific Gravity; Lubricated; Medium Hardness; Low Flow; Slip; Sunlight Resistant; UV Absorbing; Without Fillers

Uses: General Purpose; Industrial Applications; Weatherstripping

RoHS Compliant:RoHS

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  63
@Time 5.00 sec
63
@Time 0.00139 hour
Injection Molded; ASTM D2240
 65
@Time 1.00 sec
65
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 5.93 MPa860 psiFlow, Die C, 20 in/min; ASTM D412
 9.58 MPa1390 psiAcross Flow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain  2.08 MPa
@Strain 100 %
302 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 2.93 MPa
@Strain 100 %
425 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
 3.46 MPa
@Strain 300 %
502 psi
@Strain 300 %
Across Flow, Die C, 20 in/min; ASTM D412
 4.34 MPa
@Strain 300 %
630 psi
@Strain 300 %
Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 490 %490 %Flow, Die C, 20 in/min; ASTM D412
 710 %710 %Across Flow, Die C, 20 in/min; ASTM D412
Tear Strength 30.2 kN/m172 pliFlow, Die C, 20 in/min; ASTM D624
 37.2 kN/m212 pliAcross Flow, Die C, 20 in/min; ASTM D624
Compression Set  18 %
@Temperature 22.8 °C,
Time 79200 sec
18 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 87 %
@Temperature 70.0 °C,
Time 79200 sec
87 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 216 - 227 °C420 - 440 °FInjection, Melt
Rear Barrel Temperature 199 - 210 °C390 - 410 °FInjection
Middle Barrel Temperature 204 - 216 °C400 - 420 °FInjection
Front Barrel Temperature 210 - 221 °C410 - 430 °FInjection
Nozzle Temperature 216 - 227 °C420 - 440 °FInjection
Zone 1 193 - 204 °C380 - 400 °FExtrusion
Zone 2 199 - 210 °C390 - 410 °FExtrusion
Zone 3 204 - 216 °C400 - 420 °FExtrusion
Zone 4 204 - 210 °C400 - 410 °FExtrusion
Zone 5 210 - 221 °C410 - 430 °FExtrusion
Die Temperature 216 - 227 °C420 - 440 °FExtrusion
Mold Temperature 35.0 - 65.6 °C95.0 - 150 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1672 / 238163

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.