MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Rilsan® HT CESV BLACK P010-HP TL PA
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO 1183
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 300 °C
MVR (cm³/10min); ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 48.0 MPaConditioned; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 4.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 1580 MPaConditioned; ISO 527-1/-2
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 60.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 °C10°C/min; ISO 11357-1/-3
 
Descriptive Properties
FeaturesHeat stabilized or stable to heat
 Light stabilized or stable to light
 UV stabilized or stable to weather
FormPellets
Processing MethodsOther Extrusion
 Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® HT CESV BLACK P123 TL PA
Arkema Rilsan® HT CESV BLACK P010 TL PA-I
Arkema Rilsan® HT CZM 30 BLACK TLD PA-GF30
Arkema Pebax® Rnew® 35R53 SP 01 Polyether Block Amide (PEBA)
Arkema Rilsan® HT CSR13 PA-CF15

PZARKF920 / 193653

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.