MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NAECO® NAECOMET® D505F Silver Nickel Contact Material
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: For electrical contacts.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.42 g/cc0.3764 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 32 - 8432 - 8432 (annealed) - 84 (worked)
Tensile Strength, Ultimate 165 MPa23900 psiAnnealed
 220 MPa31900 psiWorked
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000181 ohm-cm0.00000181 ohm-cm(95% IACS)
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 1453 °C<= 2647 °F
Liquidus 1453 °C2647 °F
 
Component Elements PropertiesMetricEnglishComments
Nickel, Ni 5.0 %5.0 %
Silver, Ag 95 %95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NAECO® NAECOMET® D50 Silver Nickel Contact Material ASTM B693
Lucas-Milhaupt Silvaloy® A56T Brazing Alloy
NAECO® NAECOMET® D510F Silver Nickel Contact Material ASTM B693
Lucas-Milhaupt Silvaloy® A56T Flux Coated Rod Brazing Alloy
NAECO® NAECOMET® D154X Post-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3

NCMV814 / 192400

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.