MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt NORSODYNE® P 46074 Thermoset Resin
Categories: Polymer; Thermoset

Material Notes: Homogeneous system comprising a very high reactivity resin and a shrink control agent, in styrene

Appearance: NA- Light – Veiled

Main resin characteristics: Type 1130 (DIN 16946-2)

Main applications: BMC and SMC manufacture, good superficial appearance

Molding information: Pultrusion

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³
Solids Content 54 - 58 %54 - 58 %MT-CU001C
Brookfield Viscosity 1000 - 1200 cP1000 - 1200 cPsp 3 rpm 50; MT-CUT23V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FISO 75 -2A
 
Processing PropertiesMetricEnglishComments
Cure Time 6.00 - 10.0 min
@Temperature 82.0 °C
0.100 - 0.167 hour
@Temperature 180 °F
Peak, Reactivity at 82°C + 2% PBO50; MT-CU011R
Gel Time 5.00 - 7.00 min
@Temperature 82.0 °C
5.00 - 7.00 min
@Temperature 180 °F
Reactivity at 82°C + 2% PBO50; MT-CU011R
Shelf Life 9.00 Month9.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm265 - 285°CMT-CU011R; Reactivity at 82°C + 2% PBO50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9365 / 231960

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.