MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Thermoset Polyester Solventless Electrical Varnish
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Solventless Electrical Varnish

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyester Solventless Electrical Varnish". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 - 1.20 g/cc0.0336 - 0.0434 lb/in³Average value: 1.06 g/cc Grade Count:17
Viscosity 205 - 9000 cP205 - 9000 cPAverage value: 1160 cP Grade Count:17
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 3.00 - 181 kV/mm76.2 - 4600 kV/inAverage value: 79.1 kV/mm Grade Count:19
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 - 220 °C221 - 428 °FAverage value: 171 °C Grade Count:19
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 - 180 °C77.0 - 356 °FAverage value: 139 °C Grade Count:21

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyester (Thermoset) - Rigid
Overview of materials for Polyester Thermoplastic Elastomer, Glass Filled
Overview of materials for Thermoset Polyester Glass and Mineral Filled BMC
Overview of materials for Polyester Film
Overview of materials for Thermoset Polyester Glass Filled BMC

O3541 / 78222

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.