MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Firebrick SR 99 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Premium high alumina firebricks that are capable of handling very difficult applications. These premium bricks are very dense and have excellent load bearing strength at temperatures above 3000°F (1649°C) and they provide excellent thermal shock resistance. The extremely low silica content of both products make them ideal for hydrogen atmospheres.

Applications:

  • Sulphur recovery units
  • Incinerators
  • Secondary ammonia reformers

    Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.091 g/ccfired; ASTM C-134
Porosity 17 %ASTM C20
Deformation 0.00 - 0.30 %
@Temperature 1449 °C,
Time 5400 sec
ASTM C16
 0.00 - 0.30 %
@Temperature 1538 °C,
Time 5400 sec
ASTM C16
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0193 GPaambient; ASTM C 133
 0.00450 GPa
@Temperature 1538 °C
ASTM C 133
 0.00550 GPa
@Temperature 1427 °C
ASTM C 133
 0.0110 GPa
@Temperature 1260 °C
ASTM C 133
 0.0200 GPa
@Temperature 1093 °C
ASTM C 133
Compressive Strength 69.0 MPaCold Crushing Strength, ambient; ASTM C-133
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.75 W/m-K
@Temperature 1371 °C
ASTM C-201
 3.11 W/m-K
@Temperature 1093 °C
ASTM C-201
 3.68 W/m-K
@Temperature 815 °C
ASTM C-201
 4.42 W/m-K
@Temperature 538 °C
ASTM C-201
 5.61 W/m-K
@Temperature 260 °C
ASTM C-201
Melting Point 2016 °C
Maximum Service Temperature, Air <= 1760 °Chot face
Shrinkage 0.30 %
@Treatment Temp. 1760 °C,
Time 86400 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.2 %
CaO 0.10 %
Fe2O3 0.10 %
K2O+Na2O 0.20 %
MgO 0.10 %
SiO2 0.40 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6170 / 202954

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.