MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.10 - 1.90 g/ccAverage value: 1.23 g/cc Grade Count:326
 1.02 - 1.03 g/cc
@Temperature 260 - 260 °C
Average value: 1.02 g/cc Grade Count:12
Water Absorption 0.0200 - 0.700 %Average value: 0.293 % Grade Count:121
Moisture Absorption at Equilibrium 0.0200 - 0.700 %Average value: 0.128 % Grade Count:97
Water Absorption at Saturation 0.0800 - 0.500 %Average value: 0.407 % Grade Count:17
Viscosity 7.00 - 42.0 cP
@Temperature 250 - 265 °C
Average value: 208 cP Grade Count:9
 7.00 - 42.0 cP
@Load 5.00 - 5.00 kg
Average value: 208 cP Grade Count:9
 570 - 700 cP
@Temperature 260 - 260 °C
Average value: 208 cP Grade Count:4
 570 - 700 cP
@Frequency 165 - 165 Hz
Average value: 208 cP Grade Count:4
 210 - 260 cP
@Temperature 260 - 260 °C
Average value: 208 cP Grade Count:8
 210 - 260 cP
@Shear Rate 1500 - 1500 1/s
Average value: 208 cP Grade Count:8
Maximum Moisture Content 0.00200 - 0.0200Average value: 0.0190 Grade Count:28
Linear Mold Shrinkage 0.0000300 - 0.0230 cm/cmAverage value: 0.00848 cm/cm Grade Count:258
Linear Mold Shrinkage, Transverse 0.00110 - 0.0240 cm/cmAverage value: 0.00859 cm/cm Grade Count:67
Melt Flow 1.30 - 90.0 g/10 minAverage value: 17.2 g/10 min Grade Count:236
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 89.0 - 94.0Average value: 90.3 Grade Count:4
Hardness, Rockwell R 95.0 - 125Average value: 113 Grade Count:37
Hardness, Shore D 76.0 - 79.0Average value: 76.6 Grade Count:5
Ball Indentation Hardness 82.0 - 108 MPaAverage value: 99.2 MPa Grade Count:28
Tensile Strength, Ultimate 27.0 - 106 MPaAverage value: 52.1 MPa Grade Count:170
 20.0 - 20.0 MPa
@Temperature 60.0 - 60.0 °C
Average value: 20.0 MPa Grade Count:1
Tensile Strength, Yield 32.0 - 105 MPaAverage value: 54.8 MPa Grade Count:256
Elongation at Break 2.60 - 200 %Average value: 87.8 % Grade Count:278
 75.0 - 75.0 %
@Temperature 60.0 - 120 °C
Average value: 91.7 % Grade Count:1
Elongation at Yield 1.60 - 20.0 %Average value: 4.39 % Grade Count:132
 >= 10.0 %
@Temperature 60.0 - 120 °C
Average value: 10.0 % Grade Count:1
Modulus of Elasticity 0.00230 - 9.75 GPaAverage value: 2.64 GPa Grade Count:155
 1.00 - 1.40 GPa
@Temperature 60.0 - 120 °C
Average value: 1.20 GPa Grade Count:1
Flexural Yield Strength 39.0 - 160 MPaAverage value: 83.8 MPa Grade Count:272
Flexural Modulus 1.46 - 7.75 GPaAverage value: 2.38 GPa Grade Count:283
Flexural Strain at Yield 5.00 - 6.00 %Average value: 5.57 % Grade Count:9
Izod Impact 39.0 - 740 JAverage value: 389 J Grade Count:22
 90.0 - 710 J
@Temperature -40.0 - 0.000 °C
Average value: 328 J Grade Count:9
Izod Impact, Notched 0.392 - 981 J/cmAverage value: 7.14 J/cm Grade Count:208
 0.500 - 8.50 J/cm
@Temperature -40.0 - 0.000 °C
Average value: 4.04 J/cm Grade Count:79
 1.00 - 7.84532 J/cm
@Temperature -40.0 - -20.0 °C
Average value: 4.04 J/cm Grade Count:40
 1.00 - 7.84532 J/cm
@Thickness 1.57 - 6.40 mm
Average value: 4.04 J/cm Grade Count:40
Izod Impact, Unnotched 5.22 J/cm - NBAverage value: 13.3 J/cm Grade Count:37
 99.99 J/cm - NB
@Temperature -30.0 - -30.0 °C
Average value: 4.50 J/cm Grade Count:10
 4.50 - 4.50 J/cm
@Temperature -40.0 - -40.0 °C
Average value: 4.50 J/cm Grade Count:1
 4.50 - 4.50 J/cm
@Thickness 3.20 - 3.20 mm
Average value: 4.50 J/cm Grade Count:1
Izod Impact, Notched (ISO) 3.00 - 66.0 kJ/m²Average value: 40.5 kJ/m² Grade Count:107
 3.00 - 65.0 kJ/m²
@Temperature -40.0 - 40.0 °C
Average value: 28.5 kJ/m² Grade Count:100
Izod Impact, Unnotched (ISO) 30.0 kJ/m² - NBAverage value: 90.9 kJ/m² Grade Count:43
 30.0 kJ/m² - NB
@Temperature -40.0 - -30.0 °C
Average value: 85.7 kJ/m² Grade Count:43
Charpy Impact Unnotched 3.50 J/cm² - NBAverage value: 5.50 J/cm² Grade Count:62
 2.20 J/cm² - NB
@Temperature -40.0 - -20.0 °C
Average value: 7.84 J/cm² Grade Count:61
Charpy Impact, Notched 0.400 - 7.20 J/cm²Average value: 4.48 J/cm² Grade Count:114
 0.300 - 5.60 J/cm²
@Temperature -40.0 - 0.000 °C
Average value: 2.61 J/cm² Grade Count:68
Gardner Impact 36.2 - 54.0 JAverage value: 42.2 J Grade Count:14
Dart Drop, Total Energy 5.00 - 100 JAverage value: 51.1 J Grade Count:71
 3.00 - 72.0 J
@Temperature -40.0 - 0.000 °C
Average value: 43.5 J Grade Count:22
Puncture Energy 45.0 - 47.0 JAverage value: 46.3 J Grade Count:11
 55.0 - 58.0 J
@Temperature -30.0 - -30.0 °C
Average value: 57.0 J Grade Count:11
Taber Abrasion, mg/1000 Cycles 16.0 - 30.0Average value: 28.3 Grade Count:20
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 100 - 1.00e+17 ohm-cmAverage value: 1.64e+16 ohm-cm Grade Count:74
Surface Resistance 100 - 1.00e+17 ohmAverage value: 1.25e+16 ohm Grade Count:51
Dielectric Constant 2.80 - 4.00Average value: 3.20 Grade Count:50
Dielectric Strength 15.0 - 35.0 kV/mmAverage value: 23.8 kV/mm Grade Count:53
Dissipation Factor 0.000600 - 0.0300Average value: 0.00882 Grade Count:48
Arc Resistance 0.000 - 180 secAverage value: 132 sec Grade Count:22
Comparative Tracking Index 100 - 600 VAverage value: 432 V Grade Count:54
Hot Wire Ignition, HWI 7.00 - 120 secAverage value: 42.3 sec Grade Count:15
High Amp Arc Ignition, HAI 0.000 - 120 arcsAverage value: 93.6 arcs Grade Count:15
High Voltage Arc-Tracking Rate, HVTR 0.000 - 150 mm/minAverage value: 28.3 mm/min Grade Count:15
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.4 - 171 µm/m-°CAverage value: 79.6 µm/m-°C Grade Count:135
 19.8 - 122.4 µm/m-°C
@Temperature 60.0 - 138 °C
Average value: 64.6 µm/m-°C Grade Count:6
CTE, linear, Transverse to Flow 63.0 - 200 µm/m-°CAverage value: 90.7 µm/m-°C Grade Count:106
 108 - 108 µm/m-°C
@Temperature 60.0 - 138 °C
Average value: 108 µm/m-°C Grade Count:1
Specific Heat Capacity 1.78 - 1.88 J/g-°CAverage value: 1.83 J/g-°C Grade Count:12
Thermal Conductivity 0.167 - 0.200 W/m-KAverage value: 0.188 W/m-K Grade Count:42
Melting Point 219 - 271 °CAverage value: 225 °C Grade Count:35
Maximum Service Temperature, Air 90.0 - 150 °CAverage value: 115 °C Grade Count:6
Hot Ball Pressure Test 75.0 - 145 °CAverage value: 100 °C Grade Count:15
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 205 °CAverage value: 111 °C Grade Count:187
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 163 °CAverage value: 92.3 °C Grade Count:293
Vicat Softening Point 100 - 212 °CAverage value: 128 °C Grade Count:131
UL RTI, Electrical 75.0 - 140 °CAverage value: 88.3 °C Grade Count:31
UL RTI, Mechanical with Impact 75.0 - 130 °CAverage value: 87.1 °C Grade Count:31
UL RTI, Mechanical without Impact 75.0 - 140 °CAverage value: 88.9 °C Grade Count:31
Flammability, UL94 HB - 5VAGrade Count:157
Oxygen Index 20.0 - 29.0 %Average value: 21.4 % Grade Count:19
Glow Wire Test 650 - 960 °CAverage value: 782 °C Grade Count:24
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 280 °CAverage value: 119 °C Grade Count:52
Nozzle Temperature 230 - 302 °CAverage value: 261 °C Grade Count:139
Melt Temperature 170 - 330 °CAverage value: 258 °C Grade Count:215
Mold Temperature 26.7 - 110 °CAverage value: 72.0 °C Grade Count:223
Injection Velocity 200 mm/secAverage value: 200 mm/sec Grade Count:20
Roll Temperature 70.0 - 100 °CAverage value: 81.4 °C Grade Count:3
Drying Temperature 80.0 - 138 °CAverage value: 108 °C Grade Count:209
Moisture Content 0.000 - 0.0800 %Average value: 0.0198 % Grade Count:121
Dew Point -40.0 - -17.8 °CAverage value: -30.3 °C Grade Count:8
Injection Pressure 34.5 - 172 MPaAverage value: 90.4 MPa Grade Count:9
Vent Depth 0.00127 - 0.00889 cmAverage value: 0.00259 cm Grade Count:57

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polycarbonate/PET Polyester Blend

O3175a / 89079

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.