MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
Saint-Gobain Meldin® 1277 Thermoplastic Bearing Material
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Meldin 1277 has structural integrity and low deformation. This material also exhibits good electrical insulative properties and dimensional stability.

Meldin® 1000 series components are used in appliance applications due to their superior wear life and ability to operate without the need for any oils or lubricants. For scroll tip seal applications, Meldin® 1000 series materials provide some parts with superior wear resistance properties, and superior deformation properties over those of standard PTFE scroll tip seals. In vehicle systems such as transmission bearings or thrust washers, as well as fuel pump bearings, Meldin® 1000 series materials provide performance superior to metallic components. The Meldin 1000 series materials' wear resistance, coupled with their excellent chemical resistance, make them ideal materials for vehicle system components.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 g/ccASTM D792
Water Absorption 0.010 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 130 MPaASTM D 638
Elongation at Break 0.50 %ASTM D 638
Flexural Strength 170 MPaASTM D 790
Flexural Modulus 14.0 GPaASTM D790
Izod Impact, Notched 85.0 J/mASTM D 256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.50 µm/m-°CASTM E831-93
Melting Point 316 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 232 °CASTM D648
Glass Transition Temp, Tg 90.0 °CASTM D3418
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lotte Advanced Materials Infino® XP-2165BM PPS
Lotte Advanced Materials Infino® XP-2165MC PPS, 65% GF + MF
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material
Aluminum B390.0-F Die Casting Alloy
Solvay MTM® 110 series Ester Matrix Resin

PSTGQ982 / 108557

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.