Features and Applications: Compared with nylon 6 and nylon 66, nylon 610 is much softer and lower in water absorption, featured by excellent low temperature resistance and dimensional stability. Due to oil and chemicals resistance and excellent electric performance, it belongs to self-extinguishing material and can be applicable to coating of bristle like monofilaments of toothbrush and cables.Information provided by Shandong Guangyin |