MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LyondellBasell Hifax CA 182 G G12435 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax CA 182 G G12435 is an unfilled PP copolymer, with high impact resistance and good UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in G12435 color version. Prohibited Applications of Compounded Polyolefins: The use of LyondellBasell Compounded Polyolefins in the following applications is prohibited:- Air bag unit housings- Seat belt systems and mechanisms- Brake systems and mechanisms- Pedals (brake, gas, clutch)- Steering systems and mechanisms- All parts for Medical applications use.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183-1/A
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psiISO 527-1,-2
Flexural Modulus 0.950 GPa138 ksitech. A; ISO 178/A1
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -40.0 °C
2.86 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 48.0 kJ/m²
@Temperature 23.0 °C
22.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched  0.600 J/cm²
@Temperature -40.0 °C
2.86 ft-lb/in²
@Temperature -40.0 °F
ISO 179-1/1eA
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C165 °FISO 75B-1,-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications
LyondellBasell Hifax CA 60 G G12435 Polypropylene
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer
E-Polymers EFLEX® S1030 General

PEQT7191 / 218828

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.