MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik Compound VS 3000 Masterbatch
Categories: Other Engineering Material

Material Notes: Compound VS are masterbatches consisting of fumed silica and a vinyl-functional silicone polymer. They are used for producing formulations with good mechanical properties or for improving the mechanical properties of filled systems. Compound VS consists of about 30 % of surface-modified fumed silica (SiO2) and around 70 % of vinyl-functional silicone polymer.

Application: The mechanical strength of a silicone formulation depends on its silica content, i. e. tensile strength, elongation at break and tear resistance increase. At the same time, viscosity also rises substantially. This behavior is shown by the below example of a two-component addition-curing silicone. Therein the silica content of the base polymer was increased from 0 to 30 % by a stepwise replacement of Polymer VS 1000 by Compound VS 100.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/inĀ³
Filler Content 30 %30 %
Viscosity 3.00e+6 cP3.00e+6 cP
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4121.412
 
Descriptive Properties
Appearancecolorless, translucent paste
Content0.07 mmol/gVinyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Compound VS 6000 Masterbatch
Evonik Compound VS 100 Masterbatch
Wacker GenioplastĀ® Pellet P Plus Silicone Gum
Wacker GenioplastĀ® Pellet K Silicone Gum
Evonik Polymer VS 50

PEVONIL758 / 196962

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.