MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polimeros Mexicanos Rotolene® Black Plus Ultra Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Linear copolymer Medium Density Polyethylene which is fully UV8 stabilized. Available as black powder.

Applications: Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties, a high thermal resistance, zero porosity and excellent internal cure, ideal for water tanks until 2,500 L capacity. This compound meets all CONEG requirements, covering safe use in articles for direct food contact.

Information provided by Polimeros Mexicanos

Key Words: UV8 stabilized
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.330 - 0.390 g/cc0.0119 - 0.0141 lb/in³ASTM D1895-96
Density 0.939 g/cc0.0339 lb/in³ASTM D792
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Impact Test 47.5 J
@Temperature 22.2 °C
35.0 ft-lb
@Temperature 72.0 °F
0.125 in.; ARM test
 
Descriptive Properties
Dry Flow2.5 - 4 gr/minASTM D1895-96
ProcessRotational Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene
Bamberger Polymers Bapolene® 3042U Polyethylene, Rotational Molding Grade
Bamberger Polymers Bapolene® 3039U Polyethylene, Rotational Molding Grade
Polimeros Mexicanos Rotolene® High Flow Linear Medium Density Polyethylene

PMEXIC995a / 177711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.