MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik LTW-B Adhesion Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: A soft, special purpose supplementary resin with a wide compatibility range, designed to improve the initial, long-term and intercoat adhesion of paints based on vinyl chloride copolymers and in a number of other binders to metallic and mineral substrates and to certain plastics. Depending on the binder, it also improves the flexibility at normal and low temperatures

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
@Temperature 20.0 °C
DIN 51 757 / ISO 758
 1.19 g/cc
@Temperature 20.0 °C
DIN 53 4790B/ISO/R 1183
Viscosity 350 - 650 cP
@Temperature 23.0 °C
DIN EN ISO 3219
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 20 - 30[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 20.0 °CDIN 53 765
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.471Din 51 423/ISO 5661
Gardner Color Number 2.0DIN ISO 4630
 
Descriptive Properties
Hydroxyl Number (mg KOH/g)30DIN EN ISO 4629
Nonvolatile matter (%)59-61DIN EN ISO 3251

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haysite HTF Polyester, High Temp Flex
Saint-Gobain Quartzel® Fabric/Cyanate Ester Resin Composite
Saint-Gobain Chemlam® RL® RL1000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate
Sumitomo Bakelite Durez®-ter S105-55 Polyester Polyol
Sumitomo Bakelite Durez®-ter S102-27 Polyester Polyol

PHUMB109 / 81111

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.