MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Riteflex® 635 Thermoplastic Polyester Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Description: 35 Shore D Hardness 8,800 PSI flexural modulus

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183 & ASTM D792
Water Absorption 0.60 %ASTM D570
Linear Mold Shrinkage 0.0090 cm/cmASTM D955
Melt Flow 6.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35ASTM D2240 & ISO 868
Tensile Strength at Break 1920 psiASTM D638
Elongation at Break 470 %ASTM D638
Tensile Modulus 0.0600 GPa1 mm/min; ISO 527-2/1A
 8400 psiASTM D638
50% Modulus 0.00800 GPa
@Strain 50 %
ISO 527-2/1A
Flexural Strength 2.40 MPaISO 178
Flexural Modulus 0.0680 GPaISO 178
 8800 psiASTM D790
 12300 psi
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched NBASTM D256
 NB
@Temperature -40.0 °C
ASTM D256
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched NBISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
Tear Strength 715 pliASTM D624
 775 pliASTM D1004
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 5.00e+12 ohmASTM D257
Dielectric Constant 4.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 13.0 kV/mmIEC 60243-1
 310 V/milShort Term; ASTM D149
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 VASTM D3638 & IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 220 µm/m-°C
@Temperature 20.0 °C
ISO 11359-2
Melting Point 163 °CISO 11357-1,2,3 & ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 52.0 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 155 - 170 °C
Middle Barrel Temperature 170 - 180 °C
Front Barrel Temperature 170 - 180 °C
Nozzle Temperature 170 - 190 °C
Melt Temperature 170 - 190 °C
Mold Temperature 20.0 - 55.0 °C
Injection Pressure 12000 psi
Back Pressure 0.000 - 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride
Techmer ES HiFill® PVDF CF10 BK 10% Carbon Filled
BASF Elastollan® C-90A Polyester Type Polyurethane Elastomer
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer

PHCW58 / 45999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.