LG Chemical KEYFLEX BT 1040D Ester Type TPE
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyester, TP
;
Polyester Thermoplastic Elastomer
Material Notes:
Description: Injection Molding, TPC-ET, General Purpose, Medium Modulus
Application: Antenna Cover, Injection Parts for Leisure & Sports
CAS: 37282-12-5
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.13
g/cc
1.13
g/cc
ASTM D792
Water Absorption
0.70 %
@Temperature 23.0 °C,
Time 86400 sec
0.70 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Molecular Weight
458.458
g/mol
458.458
g/mol
Maximum Moisture Content
0.010
0.010
Injection Molding
0.010
0.010
Extrusion Molding
Linear Mold Shrinkage, Flow
0.0060
-
0.010
cm/cm
@Thickness 3.20 mm
0.0060
-
0.010
in/in
@Thickness 0.126 in
ASTM D955
Melt Flow
20
g/10 min
@Load 2.16 kg,
Temperature 200 °C
20
g/10 min
@Load 4.76 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
92
92
ASTM D2240
Hardness, Shore D
38
38
ASTM D2240
Tensile Strength at Break
25.5
MPa
@Thickness 2.00 mm
3700
psi
@Thickness 0.0787 in
50mm/min; ASTM D638
Elongation at Break
700 %
@Thickness 2.00 mm
700 %
@Thickness 0.0787 in
50mm/min; ASTM D638
Flexural Modulus
0.0686
GPa
@Thickness 6.40 mm
9.96
ksi
@Thickness 0.252 in
15mm/min; ASTM D790
Izod Impact, Notched
NB
@Thickness 6.40 mm,
Temperature 23.0 °C
NB
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
NB
@Thickness 6.40 mm,
Temperature -40.0 °C
NB
@Thickness 0.252 in,
Temperature -40.0 °F
ASTM D256
Tear Strength
118
kN/m
672
pli
50mm/min, at Break; ASTM D624
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+13
ohm-cm
>=
1.00e+13
ohm-cm
ASTM D257
Dielectric Strength
26.0
kV/mm
@Thickness 1.00 mm
660
kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance
180
-
240
sec
180
-
240
sec
ASTM D495
Comparative Tracking Index
600
V
600
V
Solution A; IEC 60112
Hot Wire Ignition, HWI
15
-
30
sec
@Thickness >=1.50 mm
15
-
30
sec
@Thickness >=0.0591 in
30
-
60
sec
@Thickness >=3.00 mm
30
-
60
sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI
>=
120
arcs
@Thickness 3.00 mm
>=
120
arcs
@Thickness 0.118 in
>=
120
arcs
@Thickness 1.50 mm
>=
120
arcs
@Thickness 0.0591 in
Thermal Properties
Metric
English
Comments
Melting Point
178
°C
352
°F
Deflection Temperature at 0.46 MPa (66 psi)
60.0
°C
@Thickness 6.40 mm
140
°F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical
50.0
°C
@Thickness >=1.50 mm
122
°F
@Thickness >=0.0591 in
50.0
°C
@Thickness >=3.00 mm
122
°F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact
50.0
°C
@Thickness >=1.50 mm
122
°F
@Thickness >=0.0591 in
50.0
°C
@Thickness >=3.00 mm
122
°F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact
50.0
°C
@Thickness >=1.50 mm
122
°F
@Thickness >=0.0591 in
50.0
°C
@Thickness >=3.00 mm
122
°F
@Thickness >=0.118 in
Flammability, UL94
HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
HB
@Thickness >=3.00 mm
HB
@Thickness >=0.118 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
180
-
200
°C
356
-
392
°F
Injection Molding
Middle Barrel Temperature
190
-
210
°C
374
-
410
°F
Injection Molding
Front Barrel Temperature
200
-
220
°C
392
-
428
°F
Injection Molding
Nozzle Temperature
200
-
220
°C
392
-
428
°F
Injection Molding
Zone 1
180
-
200
°C
356
-
392
°F
Extrusion Molding
Zone 2
190
-
210
°C
374
-
410
°F
Extrusion Molding
Zone 3
200
-
220
°C
392
-
428
°F
Extrusion Molding
Zone 4
200
-
220
°C
392
-
428
°F
Extrusion Molding
Adapter Temperature
200
-
220
°C
392
-
428
°F
Extrusion Molding
Die Temperature
190
-
230
°C
374
-
446
°F
Extrusion Molding
Melt Temperature
180
-
220
°C
356
-
428
°F
Extrusion Molding
180
-
220
°C
356
-
428
°F
Injection Molding
Mold Temperature
10.0
-
35.0
°C
50.0
-
95.0
°F
Injection Molding
Drying Temperature
80.0
-
90.0
°C
176
-
194
°F
Extrusion Molding
80.0
-
90.0
°C
176
-
194
°F
Injection Molding
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Extrusion Molding
3.00
-
4.00
hour
3.00
-
4.00
hour
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LG Chemical KEYFLEX BT 1028D Ester Type TPE
LG Chemical KEYFLEX BT 1245D Ester Type TPE
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Austin Novel Materials Texalan® 598A Polyether-based TPU
PLAY423 / 148433
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.