MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unifrax Fiberfrax® Rigidizer™ W Inorganic Liquid Hardener
Categories: Ceramic

Material Notes: Rigidizer™ and Rigidizer™ W, inorganic liquid hardeners, have a temperature grade rating of 1260°C (2300°F). They are generally used to increase the durability and surface erosion resistance of Fiberfrax blanket and board products. Rigidizer W hardener contains an organic wetting agent to promote saturation into the substrate, whereas Rigidizer hardener tends to remain on the material surface of the product form to which it is applied.

    Typical Applications
  • Rigidizer for surface hardening of other Fiberfrax product forms
  • Rigidizer W for saturating and rigidizing other fiberfrax product forms
  • Erosion-resistant coating for surfaces subject to high-velocity hot gases

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0433 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C30.0 µin/in-°F
Maximum Service Temperature, Air 1093 °C1999 °FRecommended Operating Temperature
 
Descriptive Properties
AppearanceBlue liquid
Approx. Coverage 1-Layer (SF/Gal)50-100
Temperature Grade (°F)2300
U.S. Coast Guard for "Incombustible Materials" Subpart 164.009X

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CUNIF043 / 97815

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.