MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cray Valley Wingtack® 10 Liquid Aliphatic C-5 Hydrocarbon Resin
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Wingtack® 10 is a liquid aliphatic resin with low color and low specific gravity. It displays excellent compatibility with many polymers, enhances tack, improves flexibility, and improves low temperature properties.

Product Highlights / Performance Properties:

  • Compatible with a wide variety of polymers, elastomers, olefins, EVA, and waxes.
  • Generally soluble in solvents having low to medium polarity
  • Improves low temperature properties
  • Low color
  • Low Tg
  • Liquid form
Suggested Applications:
  • Hot melt adhesives (HMA)
  • Pressure sensitive adhesives (PSA)
  • Sealants Plastics & Rubber
  • Coatings

Information provided by Cray Valley

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D891
Viscosity 30000 cP30000 cPE-958
Molecular Weight 370 g/mol370 g/molMn
 500 g/mol500 g/molMw
 
Thermal PropertiesMetricEnglishComments
Softening Point 10.0 °C50.0 °FE-950
Glass Transition Temp, Tg -31.0 °C-23.8 °Fmidpoint
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 1.51.5in 50% toluene; E-803
 
Descriptive Properties
AppearanceLight yellow liquid
Clarity0.95E-803a

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCRAYV032 / 316185

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.