MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Meyors Chemical HIS 70-20 Rubber Vulcanization Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Code: MSHQD -VA032-04 OT
Chemical Name: Polymeric Sulfur
Trade Name: Rubber Vulcanization Agent HIS 70-20
CAS No.: Polymeric Sulfur: 9035-99-8; Rhombic Sulfur: 7704-34-9; High pressure and hydrotreated naphthenic oil: 64742-52-5

Typical Properties: Yellow powder with slight odor, non-toxic. HIS 70-20 is not stable and at vulcanization temperatures HIS70-20 will de-polymerize to soluble sulfur. HIS 70-20 is insoluble in CS2 and in water.

Recommended Applications: HIS 70-20 is a non-blooming vulcanizing agent for unsaturated. It is polymeric sulfur and is insoluble in elastomers. so it will retard bin scorch, prevent migration of sulfur and preserve surface tack. This is important in the manufacture of tires and other plied up rubber goods. HIS 70-20 is a special grade with high thermal stability. It is used in compounds containing a relatively large sulfur loading above the solubility of sulfur in the elastomer.

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 - 1.70 g/cc
Molecular Weight 256.5 g/mol
Ash <= 0.050 %
 
Descriptive Properties
AppearanceNon-rised yellow powder
Content<0.05%Acid Content (as H2SO4)
 <0.5%Residues ( 63µm)
 >90%Insoluble sulfur content (On total S)
 19-21%Oil
 79-81%Element Sulfur
Loss on drying<0.5%
Stability>75%high temperature (105 ?15 minutes) insoluble sulfur content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMEYORS048 / 316630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.