MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® DX9305 PA 612 Dry  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: Characterization: heat- and light-stabilized

Applications: tubing systems subjected to higher temperatures, e.g., hydraulic clutch lines

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Moisture Absorption at Equilibrium 1.0 %50% RH; ISO 62
Water Absorption at Saturation 2.7 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPaISO 527-2/1A
Elongation at Break >= 50 %ISO 527-2/1A
Elongation at Yield 4.3 %ISO 527-2/1A
Tensile Modulus 2250 MPaISO 527-2/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz
ISO 60250
 4.3
@Frequency 100 Hz
ISO 60250
Dielectric Strength 23.0 kV/mmK20/P50; IEC 60423-1
Dissipation Factor 0.032
@Frequency 1e+6 Hz
IEC 60250
 0.053
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 VIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 µin/in-°F
@Temperature 23.0 - 55.0 °C
ISO 11359
Melting Point 213 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 175 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CISO 75
Vicat Softening Point 185 °C
@Load 5.10 kg
Method B; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695
 HB
@Thickness 3.20 mm
IEC 60695

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® D26 PA 612 Dry
Evonik VESTAMID® DX9325 PA 612 Dry, 40% Glass Filled

PEVONIL294 / 196498

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.