MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vikas Ecotech V-pet PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Product Description: PET is a linear thermoplastic resin that is created by the condensation of terephthalic acid and ethylene glycol. PET is a strong & reliable option especially for packaging. PET provides a long shelf life because it acts as a good barrier to elements outside of the container.

Characteristics & Usages:

  • PET has good gas and moisture barrier properties
  • PET is strong and impact-resistant
  • PET crystallinity varies from amorphous to fairly high crystalline.
  • PET is naturally colorless with a high transparency
CAS No. : 25038-59-9

Information provided by Vikas Ecotech LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.880 g/cc
Viscosity Number 0.70 - 0.74 dl/gIntrinsic
Maximum Moisture Content 0.10
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 2.0
 
Descriptive Properties
Fine<0.1%? 0.5 mm
Pellet size3 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVICAS035 / 285448

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.