Notes: Monprene SP-12950 is a general purpose thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene SP-12950 is a UV-stable, medium hardness grade suited for extrusion and injection molding. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Filled; Light Stabilized; Low Flow; Medium Density; Medium Hardness; Slip; Sunlight Resistant Uses: Consumer Applications; Gaskets; Handles; Safety Equipment; Sporting Goods; Writing Instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion; Injection Molding Information provided by Teknor Apex |