MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass/Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.20 - 1.56 g/ccAverage value: 1.36 g/cc Grade Count:35
Filler Content 30.0 - 50.0 %Average value: 45.0 % Grade Count:4
Water Absorption 0.200 - 6.00 %Average value: 1.92 % Grade Count:5
Moisture Absorption at Equilibrium 1.00 - 2.00 %Average value: 1.52 % Grade Count:8
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cmAverage value: 0.00268 cm/cm Grade Count:26
Linear Mold Shrinkage, Transverse 0.00200 - 0.0400 cm/cmAverage value: 0.00760 cm/cm Grade Count:14
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115 - 120Average value: 118 Grade Count:4
Tensile Strength, Ultimate 75.0 - 294 MPaAverage value: 194 MPa Grade Count:29
Tensile Strength, Yield 131 - 165 MPaAverage value: 149 MPa Grade Count:4
Elongation at Break 1.00 - 6.50 %Average value: 2.76 % Grade Count:31
Modulus of Elasticity 5.00 - 32.5 GPaAverage value: 15.3 GPa Grade Count:28
Flexural Yield Strength 170 - 432 MPaAverage value: 288 MPa Grade Count:24
Flexural Modulus 6.89 - 25.0 GPaAverage value: 12.5 GPa Grade Count:27
Flexural Strain at Break 1.90 - 4.40 %Average value: 3.13 % Grade Count:10
Izod Impact, Notched 0.530 - 3.20 J/cmAverage value: 1.41 J/cm Grade Count:14
Izod Impact, Unnotched 4.59 - 11.7 J/cmAverage value: 8.43 J/cm Grade Count:6
Izod Impact, Notched (ISO) 6.00 - 15.0 kJ/m²Average value: 10.3 kJ/m² Grade Count:7
 5.00 - 10.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 8.33 kJ/m² Grade Count:6
Izod Impact, Unnotched (ISO) 40.0 - 68.0 kJ/m²Average value: 57.3 kJ/m² Grade Count:7
 33.0 - 66.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 52.3 kJ/m² Grade Count:6
Charpy Impact Unnotched 4.00 - 9.00 J/cm²Average value: 6.38 J/cm² Grade Count:16
 4.00 - 5.50 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 4.75 J/cm² Grade Count:2
Charpy Impact, Notched 0.450 - 1.50 J/cm²Average value: 0.943 J/cm² Grade Count:15
 0.350 - 1.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.675 J/cm² Grade Count:2
Puncture Energy 2.30 - 2.30 J
@Temperature -30.0 - -30.0 °C
Average value: 2.30 J Grade Count:1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0500 - 1.00e+8 ohm-cmAverage value: 7.86e+6 ohm-cm Grade Count:14
Surface Resistance 100 - 1.00e+8 ohmAverage value: 6.94e+6 ohm Grade Count:19
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 - 25.0 µm/m-°CAverage value: 18.6 µm/m-°C Grade Count:4
Melting Point 249 - 275 °CAverage value: 261 °C Grade Count:12
Maximum Service Temperature, Air 110 - 220 °CAverage value: 147 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 230 - 256 °CAverage value: 248 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 210 - 260 °CAverage value: 244 °C Grade Count:21
Deflection Temperature at 8.0 MPa 190 - 210 °CAverage value: 202 °C Grade Count:5
Vicat Softening Point 200 - 255 °CAverage value: 244 °C Grade Count:10
Flammability, UL94 HBGrade Count:5
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 310 °CAverage value: 289 °C Grade Count:4
Nozzle Temperature 280 - 300 °CAverage value: 290 °C Grade Count:3
Melt Temperature 260 - 310 °CAverage value: 289 °C Grade Count:24
Mold Temperature 65.6 - 121 °CAverage value: 95.0 °C Grade Count:25
Drying Temperature 75.0 - 120 °CAverage value: 87.1 °C Grade Count:22
Moisture Content 0.0300 - 0.200 %Average value: 0.109 % Grade Count:7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 517 Polycarbonate, Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 516 Polycarbonate, Carbon Fiber Reinforced

O2529 / 78027

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.