Description: All colours, shine matt effect, compact and expanded version High quality transparent compounds for shoe industry: Available in compact (TC) and expanded (TE) version. Shine, matt surface, or shine – matt surface with slightly rubber look effect. Applications are thin shoe soles, medium thickness shoe soles and shoe soles for children. Service temperatures are between -40 to +60°C. Information provided by Uteksol d.o.o. |