MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Description

Polyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccASTM D792
Linear Mold Shrinkage 0.012 - 0.014 cm/cmASTM D955
Melt Flow 12 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPaASTM D638
Elongation at Break 25 %ASTM D638
Flexural Strength 45.0 MPaASTM D790
Flexural Modulus 2.00 GPaASTM D790
Izod Impact, Notched 30.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM D648
UL RTI, Electrical 105 °C
@Thickness 0.780 mm
UL 94
Flammability, UL94 V-0
@Thickness 0.780 mm
 V-0
@Thickness 1.57 mm
 V-0
@Thickness 3.05 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HH450MO Polypropylene
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene
Braskem H362-09RS Cast Film Polypropylene

PASHU097 / 25061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.