MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® LCBM6301 BK010 PA612-HI  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Impact Modified

Material Notes: Toughened Polyamide 612 Developed for Blow Molding

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccDAM; ISO 1183
Moisture Absorption 0.650 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 29.0 MPa50% RH; ISO 527-1/-2
 32.0 MPaDAM; ISO 527-1/-2
Elongation at Break >= 50 %50% RH; ISO 527-1/-2
 >= 50 %DAM; ISO 527-1/-2
Elongation at Yield 12 %DAM; ISO 527-1/-2
 30 %50% RH; ISO 527-1/-2
Tensile Modulus 750 MPa50% RH; ISO 527-1/-2
 1100 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.45DAM; ISO 527-1/-2
 0.4650%RH; ISO 527-1/-2
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 13.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 35.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 80.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 216 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °CDAM; ISO 75-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Descriptive Properties
Delivery formPellets
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking CodePA612-HIISO 11469
ProcessingBlow Molding
 Injection Molding
Regional AvailabilityEurope
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA612-HIISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Renol 612-01L Nylon 612, Lubricated
Avient LubriOne™ NL-30CF/15T Black Polyamide 612 (Nylon 612)
Evonik VESTAMID® DX9304 PA 612 Conditioned
Evonik VESTAMID® D26 PA 612 Dry
Evonik VESTAMID® D26 PA 612 Conditioned

PDSX5478 / 198118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.