MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nordel® NDR 37060.02 EPDM Hydrocarbon Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: NDR 37060.02 is a medium viscosity, medium ethylene EPDM grade having a moderate cure rate that is suited to applications where low modulus, good elongation, as well as heat and weather aging resistance are required. NDR 37060.02 is produced in a unique granular form that contains some carbon black.

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccASTM D297
Volatiles <= 0.40 %Total Volatiles; DuPont Dow EPRG-21
Mooney Viscosity 78
@Temperature 125 °C
ML 1 + 4; ASTM D1646
 
Descriptive Properties
Carbon Black Content (N650)30 phrDuPont Dow EPRG-2
ENB2.2 mass%ASTM D6047
Ethylene68 mass%ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ethylene Propylene Rubber (EPM, EPDM)
Dow Nordel® NDR 3722P EPDM Hydrocarbon Rubber
Dow Nordel® NDR 4820P EPDM Hydrocarbon Rubber
Dow Nordel® IP 4760P Compound
Dow Nordel® IP 4640 Molded Golf Grips

PDVG47 / 34167

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.