MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 199 X 134518 Polypropylene (PP) Glass Fiber - Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: This product has been formulated for applications that require compliance to the UL2043 standard for "Discrete Products and Their Accessories Installed in Air-Handling Spaces"

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D 792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7300 psiASTM D 638
Elongation at Break <= 5.0 %ASTM D 638
Tensile Modulus 860 ksiASTM D 638
Flexural Strength 13500 psiASTM D 790
Flexural Modulus 940 ksiASTM D 790
Izod Impact, Notched 1.30 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 8.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 - 450 °F
Mold Temperature 90.0 - 150 °F
Drying Temperature 175 °F
@Time 7200 sec
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kuraray SEPTON® 2043 Thermoplastic Rubber
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber

PQZTA26512 / 171723

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.